Compressive Strength of Mineral Trioxide Aggregate with Propylene Glycol
| Content Provider | Semantic Scholar |
|---|---|
| Author | Ghasemi, Negin Rahimi, Saeed K. Shahi, Shahriar Milani, Amin Salem Rezaei, Yashar Abbasalizadeh Nobakht, Mahnaz |
| Copyright Year | 2016 |
| Abstract | INTRODUCTION The aim of this study was to evaluate the effect of adding propylene glycol (PG) to mineral trioxide aggregate (MTA) liquid with volume ratio of 20% on the compressive strength (CS) of MTA in two time periods (4 and 21 days) after mixing. METHODS AND MATERIALS Four groups of steel cylinders (n=15) with an internal diameter of 3 and a height of 6 mm were prepared and MTA (groups 1 and 2) and MTA+PG (80% MTA liquid+20% PG) (groups 3 and 4) were placed in to the cylinders. In groups 1 and 3 the CS was evaluated after 4 days and in groups 2 and 4 after 21 days. Data were calculated using the two-ways ANOVA. The level of significance was set at 0.05. RESULTS The highest (52.22±18.92 MPa) and lowest (4.5±0.67 MPa) of CS was obtained in 21-day MTA samples and 4-day MTA+PG specimen, respectively. The effect of time and PG were significant on the CS (P<0.05). Mixing MTA with PG significantly reduced the CS; but passing the time from 4 to 21 days significantly increased the CS. CONCLUSION Considering the limitations of this study, PG had a negative effect on CS of MTA. |
| Starting Page | 325 |
| Ending Page | 328 |
| Page Count | 4 |
| File Format | PDF HTM / HTML |
| PubMed reference number | 27790264 |
| Journal | Medline |
| Volume Number | 11 |
| Alternate Webpage(s) | http://journals.sbmu.ac.ir/iej/article/download/10925/10930 |
| Journal | Iranian endodontic journal |
| Language | English |
| Access Restriction | Open |
| Content Type | Text |
| Resource Type | Article |