Loading...
Please wait, while we are loading the content...
Similar Documents
Thermal degradation behaviour of aromatic poly(ester-amide) with pendant phosphorus groups investigated by pyrolysis-GC/MS
| Content Provider | Semantic Scholar |
|---|---|
| Author | Guo, Wenjeng Leu, Wen-Tsuen Hsiao, Sheng-Huei Liou, Guey-Sheng |
| Copyright Year | 2006 |
| Abstract | Abstract The thermal stability of a novel phosphorus-containing aromatic poly(ester-amide) ODOP-PEA was investigated by thermogravimetric analysis (TGA). The weight of ODOP-PEA fell slightly at the temperature range of 300–400 °C in the TGA analysis, and the major weight loss occurred at 500 °C. The structural identification of the volatile products resulted from the ODOP-PEA pyrolysis at different temperatures was performed by pyrolysis-gas chromatography/mass spectrometry (pyrolysis-GC/MS). The P–C bond linked between the pendant DOPO group and the polymer chain disconnected first at approximately 275 °C, indicating that it is the weakest bond in the ODOP-PEA. The P–O bond in the pendant DOPO group was stable up to 300 °C. The cleavage of the ester linkage within the polymer main chain initiated at 400 °C, and the amide bond scission occurred at greater than 400 °C. The structures of the decomposition products were used to propose the degradation processes happening during the pyrolysis of the polymer. |
| Starting Page | 21 |
| Ending Page | 30 |
| Page Count | 10 |
| File Format | PDF HTM / HTML |
| DOI | 10.1016/j.polymdegradstab.2005.04.026 |
| Alternate Webpage(s) | http://homepage.ntu.edu.tw/~gsliou/FPML/Paper/2006/Polym.Degradation%20and%20Stability,%202006,%2021-30.pdf |
| Alternate Webpage(s) | https://doi.org/10.1016/j.polymdegradstab.2005.04.026 |
| Volume Number | 91 |
| Language | English |
| Access Restriction | Open |
| Content Type | Text |
| Resource Type | Article |