Effect of Types and Replacement Ratio of Alkali Activator on Compressive Strength of Ground Granulated Blast Furnace Slag Mortar
| Content Provider | Semantic Scholar |
|---|---|
| Author | Kim, Rae-Hwan Kim, Gyuyong Kim, Jong-Hee Lee, Bokyeong Cho, Bong-Suk |
| Copyright Year | 2014 |
| Abstract | In this study, effect of types and replacement ratio of alkali activator on compressive strength of ground granulated blast furnace slag mortar has been reviewed. Types of alkali activator are NaOH, Ca(OH)2, Na2SO4, and KOH. Replacement ratio of alkali activator is 7.5, 10, 12.5, and 15%, respectively. As results, under high temperature curing condition, 1 day compressive strength development with NaOH and KOH was higher than that of Ca(OH)2 and Na2SO4. Regardless of types of alkali activator, compressive strength increased with increasing pH. This can be explained by the fact that impermeable film on the surface of slag which is generated when slag contacts water has been destroyed by alkali activator, and this promotes hydration reaction. Also, 1 day age compressive strength of specimen with high temperature curing was higher than that of specimen with standard curing. 28 days age compressive strength of specimen with high temperature curing was less than or equal to that of specimen with standard curing. |
| Starting Page | 360 |
| Ending Page | 366 |
| Page Count | 7 |
| File Format | PDF HTM / HTML |
| DOI | 10.14190/JRCR.2014.2.4.360 |
| Volume Number | 2 |
| Alternate Webpage(s) | http://ocean.kisti.re.kr/downfile/volume/kfcr/GSJHDK/2014/v2n4/GSJHDK_2014_v2n4_360.pdf |
| Alternate Webpage(s) | https://doi.org/10.14190/JRCR.2014.2.4.360 |
| Language | English |
| Access Restriction | Open |
| Content Type | Text |
| Resource Type | Article |